Ferro Feldspar No. 10

Alternate Names: Ferro Feldspar #10

Description: Legacy feldspar

Oxide Analysis Formula Tolerance
K2O 9.84% 0.71
Na2O 2.59% 0.29
Al2O3 14.64% 0.98
SiO2 68.83% 7.83
LOI 4.10%n/a
Oxide Weight 655.80
Formula Weight 683.84