Description: SOUTH CAROLINA KAOLIN
| Oxide | Analysis | Formula | Tolerance |
|---|
| Materials |
McNamee Kaolin
|
| Materials |
Dixie Clay
|
| Materials |
Peerless 2 Kaolin
|
| Materials |
Langford Kaolin
|
| Materials |
Bilt-Cote Kaolin
|
| Materials |
Peerless 3 Kaolin
|
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |