Dixie Clay

Description: SOUTH CAROLINA KAOLIN

Notes

The company promotes it as a small particle size material and they target it at rubber manufacturers. Its surface area is about 26 square meters per gram compared to peerless which is about 16 square meters per gram.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials McNamee Kaolin
Materials PAR Kaolin
Materials Peerless 2 Kaolin
Materials Langford Kaolin
Materials Bilt-Cote Kaolin
Materials Peerless 3 Kaolin
Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.
URLs https://www.vanderbiltminerals.com/resources/Minerals_and_Chemical_for_Ceramics_and_Refractories_web.pdf
Vanderbilt Minerals for Ceramics Technical Sheet
Includes Vansil, Pyrax, Peerless, Dixie, Veegum, Vanzan, Darvan.

Data

GE Brightness 70
% Passing 325 Mesh Wet 99.8%
Moisture Content - Powder 1% Max
Median Particle Size (Microns) 0.2 microns