1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

AD Enamel

Oxide Analysis Formula Tolerance
CaO 0.30% 0.02
K2O 0.20% 0.01
MgO 0.30% 0.03
Na2O 0.30% 0.02
TiO2 1.50% 0.06
Al2O3 30.10% 1.00
SiO2 55.30% 3.12
Fe2O3 1.50% 0.03
LOI 10.50%n/a
Oxide Weight 303.29
Formula Weight 338.87

Related Information

Data

Dry M.O.R. (50% Silica) 851C