Lunday Kaolin

Description: Extinct kaolin from Harris Mining Co.

Oxide Analysis Formula Tolerance
SiO2 47.29% 2.21
Al2O3 36.32% 1.00
Fe2O3 0.98% 0.02
TiO2 0.06% -
K2O 1.27% 0.04
Na2O 0.26% 0.01
LOI 13.60%n/a
Oxide Weight 242.03
Formula Weight 280.12

Related Information

Links

Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.