Alternate Names: Frit CC262
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 2.40% | 0.12 | |
| ZnO | 9.20% | 0.88 | |
| Oxide Weight | 90.15 | ||
| Formula Weight | 90.15 | ||
One source specified SiO2:Al2O3 ratio of: 11.04
Alkalies: less than 5%
CaO: 5-10-%
MgO: less than 5%
Al2O3: 5-10%
SiO2: 5-10%
SiO2: More than 50%
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.2 |
|---|
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk