Solargil Frit FR9

Description: Zircon frit

Oxide Analysis Formula Tolerance
CaO 6.09% 0.32
Na2O 5.05% 0.24
K2O 5.11% 0.16
ZnO 7.73% 0.28
B2O3 8.03% 0.34
ZrO 8.36% 0.23
Al2O3 13.15% 0.38
SiO2 46.48% 2.28
Oxide Weight 294.80
Formula Weight 294.80

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 68.6 x 10-7 C (Appen)
Frit Softening Point 940-980C
By Tony Hansen