Cresta BB

Alternate Names: Gulgong clay

Oxide Analysis Formula Tolerance
CaO 0.10% 0.01
K2O 0.20% 0.01
MgO 0.50% 0.05
Na2O 0.30% 0.02
TiO2 1.00% 0.05
Al2O3 25.60% 1.00
SiO2 63.10% 4.18
Fe2O3 0.61% 0.02
LOI 8.60%n/a
Oxide Weight 364.21
Formula Weight 398.48

Notes

The mine at Gulgong, NSW, Australia, produced a white, plastic raw clay that was used by many people (and manufacturers) to make clay bodies of many types (especially stoneware). It was prized as the best combination of whiteness and plasticity available in the country. It has a very low iron content and very low concentration of fluxes.

In 2015 it was determined to be uneconomic by the manufacturer so not more stockpiles have been made. In addition the last of the stockpiled Gulgong clay appears to be slightly different (less white and plastic). As a result companies had to reformulate their bodies, often the replacement being of lower quality.

Related Information

Gulgong Clay from NSW, Australia


This picture has its own page with more detail, click here to see it.

Prized for its whiteness and plasticity. A base for many stonewares.


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy