| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 59.37% | 2.13 | |
| TiO2 | 0.27% | 0.01 | |
| P2O5 | 1.65% | 0.03 | |
| Al2O3 | 8.41% | 0.18 | |
| B2O3 | 0.39% | 0.01 | |
| Fe2O3 | 1.71% | 0.02 | |
| MgO | 0.73% | 0.04 | |
| Na2O | 23.50% | 0.82 | |
| CaO | 1.93% | 0.07 | |
| K2O | 2.04% | 0.05 | |
| Oxide Weight | 215.13 | ||
| Formula Weight | 215.13 | ||
Described by Bob Hay in Ceramics Monthly 9/1980.
See also "Pottery in India" by Gurcharan Singh, 1979.