Degussa Frit 90167

Alternate Names: Alkaliborfritte

Description: High alkali borosilicate frit

Oxide Analysis Formula Tolerance
SiO2 43.93% 1.80
B2O3 16.96% 0.60
Al2O3 8.28% 0.20
CaO 2.28% 0.10
Na2O 11.33% 0.45
K2O 17.21% 0.45
Oxide Weight 246.23
Formula Weight 246.23

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 150 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 455C
Heating Microscope Analysis for Frits 646C
Heating Microscope Analysis for Frits 740C