Esan Feldspar

Alternate Names: ESF501FG

Description: Turkish Soda Feldspar

Oxide Analysis Formula Tolerance
SiO2 70.00% 6.66
Al2O3 18.00% 1.01
Fe2O3 0.05% -
TiO2 0.05% -
CaO 0.30% 0.03
MgO 0.20% 0.03
K2O 0.30% 0.02
Na2O 10.00% 0.92
LOI 0.30%n/a
Oxide Weight 565.84
Formula Weight 567.54

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

Data

Ultimate Particle Size Distribution +200 3.50 +100 13.00 +74 24.50 +63 6.00 +45 13.00 -45 40.00