RC4 Vitreous

Oxide Analysis Formula Tolerance
CaO 1.00% 0.08
MgO 0.20% 0.02
K2O 1.30% 0.06
Na2O 2.80% 0.21
TiO2 0.29% 0.02
Al2O3 22.00% 1.00
SiO2 71.40% 5.51
Fe2O3 0.65% 0.02
LOI 0.30%n/a
Oxide Weight 461.97
Formula Weight 463.36

Related Information

Links

Materials RC10 Vitreous
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

Data

Bulk Density g/cc (Packed) 1.4
Hardness (Moh) 7
Ultimate Particle Size Distribution >71 micron: 1.6%
Density (Specific Gravity) 2.6
pH for dry powder 7-8