Alternate Names: Feldspar Soda F7/SE
Description: Soda Feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.55% | 0.05 | |
| MgO | 0.05% | 0.01 | |
| K2O | 0.28% | 0.02 | |
| Na2O | 10.20% | 0.92 | |
| TiO2 | 0.06% | - | |
| Al2O3 | 17.50% | 0.96 | |
| SiO2 | 70.80% | 6.60 | |
| Fe2O3 | 0.12% | - | |
| LOI | 0.36% | n/a | |
| Oxide Weight | 557.66 | ||
| Formula Weight | 559.67 | ||
| Minerals |
Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO |
| Minerals |
Na-Feldspar
Most common feldspars contain both sodium and potassium. The term Na-Feldspar designates one where t |
| Materials |
Soda Feldspar
A feldspar having a KNaO content that predominates in sodium. |
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |
| Bulk Density g/cc (Packed) | 1.2 |
|---|---|
| Hardness (Moh) | 6.5 |
| Ultimate Particle Size Distribution | >71 micron: 1% |
| Density (Specific Gravity) | 2.65 |
| pH for dry powder | 8-9 |