A-3 Feldspar

Alternate Names: A3 Feldspar, Kona A-3 Feldspar, Kona A3 Feldspar

Description: potash feldspar

Oxide Analysis Formula Tolerance
CaO 0.40% 0.05
K2O 7.51% 0.53
Na2O 4.00% 0.43
Al2O3 16.30% 1.06
SiO2 71.63% 7.87
Fe2O3 0.07% -
LOI 0.09%n/a
Oxide Weight 660.04
Formula Weight 660.63

Notes

No longer available.

Related Information

Links

Materials Potash Feldspar
A feldspar having a KNaO content that predominates in potassium.
Materials Soda Feldspar
A feldspar having a KNaO content that predominates in sodium.
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy