Mica - musc

Description: From Ron Roy's MDT

Oxide Analysis Formula Tolerance
CaO 0.50% 0.06
MgO 0.69% 0.12
K2O 9.77% 0.73
Na2O 0.80% 0.09
TiO2 0.65% 0.06
Al2O3 33.20% 2.28
SiO2 47.74% 5.57
Fe2O3 2.03% 0.09
LOI 4.80%n/a
Oxide Weight 668.62