Low Melt Spodumene

Alternate Names: Low Melt Spod (Hank)

Description: From Ron Roy's materials table

Oxide Analysis Formula Tolerance
Li2O 7.55% 0.77
K2O 0.31% 0.01
Na2O 0.31% 0.02
P2O5 9.32% 0.20
Al2O3 27.94% 0.84
SiO2 54.33% 2.76
Fe2O3 0.21% -
MnO2 0.03% -
Oxide Weight 305.51
Formula Weight 305.51

Related Information

Links

Materials Foote Spodumene
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.