1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

New FHC

Oxide Analysis Formula Tolerance
CaO 0.21% 0.02
MgO 0.12% 0.01
K2O 0.78% 0.03
Na2O 0.20% 0.01
TiO2 0.84% 0.04
Al2O3 24.95% 1.00
SiO2 60.34% 4.10
Fe2O3 1.42% 0.04
MnO 0.03% -
LOI 11.11%n/a
Oxide Weight 363.40
Formula Weight 408.82