| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Fe2O3 | 1.61% | 0.05 | |
| SiO2 | 66.75% | 5.49 | |
| Al2O3 | 20.65% | 1.00 | |
| TiO2 | 0.53% | 0.03 | |
| Na2O | 0.55% | 0.04 | |
| K2O | 0.68% | 0.04 | |
| MgO | 0.51% | 0.06 | |
| CaO | 0.50% | 0.04 | |
| LOI | 8.21% | n/a | |
| Oxide Weight | 453.34 | ||
| Formula Weight | 493.89 | ||