Pemco Frit P-3T355

Alternate Names: 3T355,3T-355

Oxide Analysis Formula Tolerance
MgO 0.99% 0.09
CaO 0.65% 0.04
K2O 5.55% 0.21
Na2O 10.88% 0.62
ZnO 0.92% 0.04
ZrO2 15.67% 0.45
Al2O3 8.53% 0.30
B2O3 14.97% 0.76
SiO2 41.82% 2.47
Oxide Weight 354.72
Formula Weight 354.72

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.