Virginia Kyanite

Oxide Analysis Formula Tolerance
SiO2 37.46% 1.06
Fe2O3 0.91% 0.01
Al2O3 59.90% 1.00
TiO2 0.92% 0.02
Na2O 0.20% 0.01
K2O 0.20% -
MgO 0.06% -
CaO 0.05% -
LOI 0.29%n/a
Oxide Weight 169.77
Formula Weight 170.27

Related Information

Links

Materials Mullite
A highly refractory low-expansion alumino-silicate crystal formed naturally only rarely but produced industrially and within fired kaolin bodies.
Materials Pyrophyllite
A refractory aluminum silicate mineral often used in clay body recipes to lower thermal expansion, control fired maturity, mullite development catalyst, etc.
Materials Kyanite
A refractory aluminum silicate mineral notable for low thermal expansion and one-way volume expansion as it converts to mullite at high temperatures.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy