| Monthly Tech-Tip | No tracking! No ads! | |
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.05% | - | |
| MgO | 0.10% | 0.01 | |
| K2O | 0.20% | 0.01 | |
| Na2O | 0.08% | - | |
| TiO2 | 1.65% | 0.05 | |
| Al2O3 | 38.50% | 1.00 | |
| SiO2 | 45.00% | 1.98 | |
| Fe2O3 | 0.55% | 0.01 | |
| LOI | 13.60% | n/a | |
| Oxide Weight | 228.19 | ||
| Formula Weight | 264.11 | ||
An intermediate-grained airfloated Kaolin suitable for use as a filler and pigment in a wide variety of industrial applications including soft rubber, plastics, ceiling tile, adhesives and paper products.
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| Surface Area (m2/gm) | 13.5 |
|---|
| By Tony Hansen Follow me on ![]() | ![]() |