Frit RCG 2430

Alternate Names: F RCG 2430, RCG2430, RCG-2430

Oxide Analysis Formula Tolerance
SiO2 56.20% 2.62
B2O3 13.20% 0.53
Al2O3 9.70% 0.27
Na2O 6.40% 0.29
K2O 0.60% 0.02
CaO 13.90% 0.69
Oxide Weight 279.82
Formula Weight 279.82

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3124
A commonly available calcium borosilicate frit.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.