M70 Mullite

Description: Needle shaped interwoven mullite

Oxide Analysis Formula Tolerance
Na2O 0.10% -
K2O 0.10% -
MgO 0.30% 0.01
CaO 0.30% 0.01
Fe2O3 1.30% 0.01
TiO2 2.50% 0.05
SiO2 36.00% 1.02
Al2O3 60.00% 1.00
Oxide Weight 171.02
Formula Weight 171.02

Notes

Also make M60 which is less pure.

Related Information

Links

Materials Mullite
A highly refractory low-expansion alumino-silicate crystal formed naturally only rarely but produced industrially and within fired kaolin bodies.
Typecodes Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy