Magnabrite

Alternate Names: Magnabrite T

Description: Magnesium Aluminum Silicates

Oxide Analysis Formula Tolerance
SiO2 70.93% 3.42
Al2O3 10.33% 0.29
MgO 9.17% 0.66
Fe2O3 1.51% 0.03
CaO 5.23% 0.27
Na2O 1.02% 0.05
K2O 0.76% 0.02
LOI 5.10%n/a
Oxide Weight 286.57
Formula Weight 301.97

Notes

Highly purified blend of white smectite clays supplied as small flakes. Used when an inorganic, thixotropic material is desired to disperse pigments, retard settling, impart body plasticity or stabilize emulsions. It is a nonmigrating binder that delivers high yield values that enable the suspension of high-density pigments and particles.

Used to ease of dispersion, high viscosity, excellent stability and rheology.

Related Information

Links

Materials Hectalite 200
Materials Veegum
A clay of incredibly small particle size. It has the highest plasticity of any known clay and acts as a suspending and gelling agent in slurries.
Materials Hectabrite
White magnesium-rich surface-modified highly purified sodium hectorite clay 4-5 times more efficient than raw bentonite.
URLs http://www.colloid.com/ISG/TechData/Magnabrite%20T%20Tech%20Sheet.pdf