Potterycrafts Frit P2958

Alternate Names: PotteryCrafts Frit 2958

Oxide Analysis Formula Tolerance
CaO 5.30% 0.42
K2O 1.34% 0.06
Na2O 7.08% 0.51
Al2O3 12.07% 0.53
B2O3 16.21% 1.04
SiO2 57.99% 4.33
Oxide Weight 448.60
Formula Weight 448.60

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.