Description: Netherlands, Flanders area (Ferro?)
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 4.77% | 0.21 | |
| SiO2 | 52.82% | 2.17 | |
| B2O3 | 10.73% | 0.38 | |
| Na2O | 19.17% | 0.76 | |
| Al2O3 | 11.52% | 0.28 | |
| K2O | 0.99% | 0.03 | |
| Oxide Weight | 247.08 | ||
| Formula Weight | 247.08 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |