Ferro Frit 3043

Description: Netherland, Flanders area (Ferro?)

Oxide Analysis Formula Tolerance
CaO 7.18% 0.43
B2O3 6.42% 0.31
SiO2 54.20% 3.03
Al2O3 6.07% 0.20
Na2O 2.03% 0.11
K2O 3.93% 0.14
MgO 0.24% 0.02
PbO 19.93% 0.30
Oxide Weight 335.91
Formula Weight 335.91

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.