Frit 1202

Description: Alkali high calcium low boron low alumina frit

Oxide Analysis Formula Tolerance
K2O 19.60% 0.50
Na2O 5.20% 0.20
ZnO 10.20% 0.30
Al2O3 6.40% 0.15
SiO2 50.00% 1.99
B2O3 8.70% 0.30
Oxide Weight 239.91
Formula Weight 239.91

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.