Frit 1210

Description: Zinc alkali opacified alumina silicate frit

Oxide Analysis Formula Tolerance
CaO 4.00% 0.28
B2O3 19.70% 1.11
Al2O3 3.90% 0.15
SiO2 48.50% 3.16
ZnO 6.30% 0.30
Na2O 2.40% 0.15
K2O 4.80% 0.20
Li2O 0.50% 0.07
ZrO2 9.80% 0.31
Oxide Weight 391.55
Formula Weight 391.55

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.