Frit 1213

Description: Barium iron borosilicate low alumina frit

Oxide Analysis Formula Tolerance
BaO 18.80% 0.51
CaO 2.70% 0.20
Li2O 0.50% 0.07
Na2O 1.90% 0.13
ZnO 2.00% 0.10
Al2O3 3.70% 0.15
B2O3 17.00% 1.01
SiO2 33.70% 2.31
Fe2O3 19.60% 0.50
Oxide Weight 411.52
Formula Weight 411.52

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.