Dankwean Red Clay

Description: Thai clay from Dankwean, Korat

Oxide Analysis Formula Tolerance
TiO2 1.04% 0.05
Fe2O3 6.81% 0.17
CaO 0.06% -
MgO 0.73% 0.07
Na2O 0.15% 0.01
K2O 1.33% 0.06
Al2O3 25.63% 1.00
SiO2 54.69% 3.62
LOI 9.50%n/a
Oxide Weight 359.93
Formula Weight 397.71