1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Dankwean Sandy Clay

Description: Dankwean Village Sandy Clay

Oxide Analysis Formula Tolerance
Na2O 0.55% 0.07
MgO 0.26% 0.05
CaO 0.31% 0.04
Fe2O3 3.86% 0.18
TiO2 0.83% 0.08
K2O 0.87% 0.07
Al2O3 13.83% 1.00
SiO2 74.53% 9.15
LOI 4.96%n/a
Oxide Weight 700.95
Formula Weight 737.53