Volclay SPV 200 Bentonite

Description: SODIUM BENTONITE

Oxide Analysis Formula Tolerance
CaO 1.30% 0.17
K2O 0.30% 0.02
MgO 2.70% 0.51
Al2O3 20.69% 1.53
SiO2 69.56% 8.73
Fe2O3 4.85% 0.23
Na2O 2.43% 0.30
Oxide Weight 768.25
Formula Weight 768.25

Notes

See HPM-20 for microfine version of this.

A selectively mined and processed, high quality sodium bentonite.
It is used for suspending, emulsifying, and as a binding agent for industrial products where a dry 200 mesh particle size is required. It contains small portions of feldspar, calcite and quartz.
Moisture is 12% as shipped.
Dry PSD: Minimum 65% finer that 200 mesh (74 microns)
Wet PSD: Minimum 94% finer that 200 mesh (74 microns)
Minimum 92% finer than 325 mesh (44 microns)
pH: 2% solids: 8.5-10.5

Viscosity: 8-30 cps @ 6.25% solids

Related Information

Links

Materials HPM-20 Volclay Bentonite
Materials Bentonite
Bentonite can make a clay body instantly plastic, only 2-3% can have a big effect. It also suspends slurries so they don't settle out and slows down drying.
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy