1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Cerium Oxide

Alternate Names: CeO2, Cerium Dioxide

Oxide Analysis Formula Tolerance
CeO2 100.00% 1.00
Oxide Weight 172.11
Formula Weight 172.11

Notes

A colorant used in ceramic glazes. It is a powerful flux. Commercial products have fairly high purity.
Can be used as a polishing and descratching agent for glass.
Also available as a carbonate (CeCO3).

Related Information

Links

URLs http://www.kemcointernational.com/CeriumOxide.htm
Kemco International - Cerium Description
URLs http://en.wikipedia.org/wiki/Cerium_Oxide
Cerium oxide at Wikipedia
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
Oxides CeO2 - Cerium Oxide
Minerals Bastnäsite
A cerium cortaining carbonate-fluoride mineral.
Minerals Monazite
A cerium containing phosphate mineral.

Data

Hardness (Moh) 6
Frit Softening Point 2500C
Density (Specific Gravity) 7.3
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy