Barium Feldspar

Alternate Names: Celsian

Oxide Analysis Formula Tolerance
BaO 40.84% 1.00
Al2O3 27.16% 1.00
SiO2 32.01% 2.00
Oxide Weight 375.40
Formula Weight 375.40

Related Information

Links

URLs http://www.webmineral.com/data/Celsian.shtml
Celsian at Webmineral.com
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.