Matthey Calcium Borate Frit

Oxide Analysis Formula Tolerance
CaO 26.99% 1.00
K2O 0.05% -
Na2O 0.03% -
B2O3 50.57% 1.51
Al2O3 4.97% 0.10
SiO2 17.40% 0.60
Oxide Weight 207.44
Formula Weight 207.44

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Calcium Borate
Materials PotteryCrafts Frit P2954
A calcium borate frit (with extremely high boron).
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.