1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Wolcon

Oxide Analysis Formula Tolerance
CaO 36.45% 0.84
K2O 0.26% -
MgO 4.78% 0.15
Na2O 0.03% -
Al2O3 0.77% 0.01
P2O5 0.20% -
SiO2 50.29% 1.08
Fe2O3 0.26% -
LOI 6.97%n/a
Oxide Weight 120.36