Vanadium Pentoxide

Alternate Names: Vanadium (V) Oxide

Oxide Analysis Formula Tolerance
V2O5 100.00% 1.00
Oxide Weight 181.90
Formula Weight 181.90

Notes

A coloring agent that produces yellows, especially when in combination with tin oxide. It is also a strong flux.

Related Information

Links

Hazards Vanadium and Compounds Toxicology
Typecodes Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials.
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
URLs http://en.wikipedia.org/wiki/Vanadium(V)_oxide
Vanadium and Wikipedia
Oxides V2O5 - Vanadium Pentoxide

Data

Frit Softening Point 690C M
Density (Specific Gravity) 3.40
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 