| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.53% | 0.01 | |
| K2O | 0.02% | - | |
| MgO | 31.63% | 0.99 | |
| Na2O | 0.09% | - | |
| TiO2 | 0.02% | - | |
| Al2O3 | 0.41% | 0.01 | |
| SiO2 | 61.78% | 1.29 | |
| Fe2O3 | 0.05% | - | |
| LOI | 5.47% | n/a | |
| Oxide Weight | 118.76 | ||
| Formula Weight | 125.63 | ||