Stone C

Oxide Analysis Formula Tolerance
CaO 0.12% 0.01
K2O 10.16% 0.73
MgO 0.07% 0.01
Na2O 2.23% 0.24
Al2O3 21.31% 1.41
SiO2 62.66% 7.06
Fe2O3 0.25% 0.01
LOI 3.20%n/a
Oxide Weight 655.39
Formula Weight 677.05