| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.07% | 0.01 | |
| K2O | 5.44% | 0.23 | |
| MgO | 0.25% | 0.02 | |
| Na2O | 0.23% | 0.01 | |
| TiO2 | 0.13% | 0.01 | |
| Al2O3 | 25.35% | 1.00 | |
| SiO2 | 63.24% | 4.23 | |
| Fe2O3 | 0.27% | 0.01 | |
| LOI | 4.55% | n/a | |
| Oxide Weight | 382.17 | ||
| Formula Weight | 400.39 | ||