Stone A

Oxide Analysis Formula Tolerance
CaO 0.18% 0.01
K2O 4.81% 0.19
MgO 0.20% 0.02
Na2O 0.13% 0.01
TiO2 0.13% 0.01
Al2O3 28.11% 1.00
SiO2 62.40% 3.77
Fe2O3 0.21% -
LOI 4.65%n/a
Oxide Weight 348.96
Formula Weight 365.98