Steetley Feldspar

Description: AUSTRALIAN FELDSPAR

Oxide Analysis Formula Tolerance
CaO 0.30% 0.03
K2O 10.30% 0.62
MgO 0.10% 0.01
Na2O 3.60% 0.33
Al2O3 18.00% 1.01
SiO2 67.00% 6.36
Fe2O3 0.30% 0.01
Oxide Weight 568.38
Formula Weight 568.38

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.