C-85-RK Bauxite

Oxide Analysis Formula Tolerance
CaO 0.25% 0.01
K2O 0.10% -
MgO 0.25% 0.01
TiO2 3.80% 0.05
Al2O3 88.99% 1.00
SiO2 5.00% 0.10
Fe2O3 1.50% 0.01
Oxide Weight 114.49
Formula Weight 114.49

Related Information

Links

Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.