C-85 Bauxite

Oxide Analysis Formula Tolerance
CaO 0.10% -
K2O 0.10% -
MgO 0.10% -
Na2O 0.10% -
TiO2 3.52% 0.05
Al2O3 88.44% 1.00
SiO2 6.03% 0.12
Fe2O3 1.60% 0.01
Oxide Weight 115.32
Formula Weight 115.32

Related Information

Links

Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.