C-6 Feldspar

Description: SODA FELDSPAR

Oxide Analysis Formula Tolerance
CaO 0.70% 0.07
K2O 5.19% 0.31
MgO 0.06% 0.01
Na2O 6.89% 0.62
Al2O3 18.48% 1.01
SiO2 68.43% 6.32
Fe2O3 0.06% -
LOI 0.24%n/a
Oxide Weight 553.91
Formula Weight 555.24