| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.03% | - | |
| K2O | 3.30% | 0.11 | |
| MgO | 0.14% | 0.01 | |
| Na2O | 0.07% | - | |
| TiO2 | 0.19% | 0.01 | |
| Al2O3 | 32.68% | 1.00 | |
| SiO2 | 52.60% | 2.73 | |
| Fe2O3 | 1.33% | 0.03 | |
| LOI | 9.66% | n/a | |
| Oxide Weight | 281.97 | ||
| Formula Weight | 312.12 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |