BPS Standard Borax Frit

Description: Borax Frit

Oxide Analysis Formula Tolerance
CaO 14.22% 0.60
K2O 1.57% 0.04
MgO 0.17% 0.01
Na2O 9.02% 0.35
B2O3 17.94% 0.61
Al2O3 7.63% 0.18
SiO2 49.46% 1.96
Oxide Weight 238.23
Formula Weight 238.23

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials PotteryCrafts Frit P2953
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.