BPS Low Expansion Frit

Description: High calcium boro aluminum silicate frit

Oxide Analysis Formula Tolerance
CaO 10.96% 0.76
K2O 0.73% 0.03
MgO 0.10% 0.01
Na2O 3.19% 0.20
B2O3 18.25% 1.02
Al2O3 14.42% 0.55
SiO2 52.36% 3.39
Oxide Weight 389.07
Formula Weight 389.07

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.