BPS Cornish Stone

Oxide Analysis Formula Tolerance
CaO 1.49% 0.19
K2O 4.52% 0.35
MgO 0.14% 0.02
Na2O 3.48% 0.41
TiO2 0.06% 0.01
Al2O3 15.49% 1.11
P2O5 0.48% 0.02
SiO2 74.22% 8.99
Fe2O3 0.13% 0.01
Oxide Weight 728.33
Formula Weight 728.33